1四川会东磷矿石反浮选试验一、原矿性质:该磷矿石为原生矿,矿石主要呈灰黑色,含少量灰白色,原矿氧化镁含量较高。二、原矿样多元素分析:元素P2O5MgOFe2O3Al2O3CaOSiO2MnOF酸不熔物含量%27.205.370.771.2346.852.400.352.742.82三、试验方案:将矿石破碎至-2mm以下,充分混匀,经磨矿分样后进行一次粗反开路浮选流程试验。四、试验药剂及配制浓度:名称2#油H2SO4H3PO4H969浓度%原液1052五、试验条件:1.试验温度:室温19℃2.试验浓度:33±1%3.试验细度:-200目占61.47%、73.00%、87.88%4.试验PH值:5-65.试验时间:10分钟6.试验线速度:4.66m/s2六、试验流程:试验流程为一次粗反开路浮选流程,见下图:原矿精矿尾矿粗反七、试验数据:1.试验(一):a.原矿筛析:-200目含量为61.47%(见下表.1.)表.1.粒级(目)产率%P2O5%MgO%回收率备注P2O5%MgO%+10011.0130.171.6412.263.71+100目粒级P2O5品位30.17%最高,磷矿物结晶较粗;-320目粒级部分过磨。-100+20027.5229.904.0930.3923.30-200+32028.4427.655.4129.0331.75-320+40021.1123.615.1918.3222.68-40011.9222.717.5610.0018.56Σ100.0027.084.85100.00100.003b.试验结果:(见下表.2.细度-200目占61.47%)表.2.药剂制度产品产率%P2O5%MgO%回收率P2O5%MgO%2#油:4滴H2SO4:1.0Kg/t.αH3PO4:4.0Kg/t.αH969:3.0Kg/t.α精矿69.9133.752.2786.1929.72尾矿30.0912.5612.4813.8170.28原矿100.0027.375.35100.00100.002#油:4滴H2SO4:1.0Kg/t.αH3PO4:4.0Kg/t.α2XP-64:3.0Kg/t.α精矿65.1534.651.6783.0422.20尾矿34.8513.2310.9716.9677.80原矿100.0027.184.91100.00100.002#油:4滴H2SO4:1.0Kg/t.αH3PO4:4.0Kg/t.αH969:2.0Kg/t.α精矿70.5734.151.9787.6028.90尾矿29.4311.6011.6312.4071.10原矿100.0027.514.81100.00100.002.试验(二)a.原矿筛析:-200目含量为73.00%(见下表.3.)表.3.粒级(目)产率%P2O5%MgO%回收率P2O5%MgO%+1005.0031.162.855.662.92-100+20022.0031.522.9125.1313.33-200+32036.0028.374.2437.0231.88-320+40026.0024.576.4223.1734.79-40011.0022.617.469.0217.08Σ100.0027.584.80100.00100.004b.试验结果:(见下表.4.)表.4.药剂制度产品产率%P2O5%MgO%回收率P2O5%MgO%2#油:4滴H2SO4:0.5Kg/t.αH3PO4:3.0Kg/t.αH969:0.5Kg/t.α精矿78.7032.213.0992.0544.34尾矿21.3010.2714.317.9555.66原矿100.0027.545.48100.00100.002#油:4滴H2SO4:1.0Kg/t.αH3PO4:4.0Kg/t.αH969:3.0Kg/t.α精矿61.4534.691.2178.5613.68尾矿38.5515.1112.1921.4486.32原矿100.0027.145.41100.00100.002#油:4滴H2SO4:0.5Kg/t.αH3PO4:5.0Kg/t.αH969:1.5Kg/t.α精矿65.7635.081.3184.5418.26尾矿34.2412.3211.2315.4681.74原矿100.0027.294.71100.00100.002#油:4滴H2SO4:1.0Kg/t.αH3PO4:6.0Kg/t.αH969:1.5Kg/t.α精矿72.1634.051.7189.7023.70尾矿27.8410.1214.2110.3076.30原矿100.0027.395.19100.00100.002#油:4滴H2SO4:1.0Kg/t.αH3PO4:7.0Kg/t.αH969:1.5Kg/t.α精矿70.6934.941.7389.0422.51尾矿29.3110.3614.3310.9677.49原矿100.0027.745.42100.00100.003.试验(三):a.原矿筛析:-200目含量为87.88%(见下表.5.)5表.5.粒级(目)产率%P2O5%MgO%回收率P2O5%MgO%+1001.0123.343.990.930.66-100+20011.1125.354.0210.867.39-200+32038.8929.084.9943.5831.86-320+40027.2723.367.5424.5533.83-40021.7223.987.3820.0826.26Σ100.0025.956.09100.00100.00b.试验结果:(-200目占87.88%,见下表.6.)表.6.药剂制度产品产率%P2O5%MgO%回收率P2O5%MgO%2#油:4滴H2SO4:1.0Kg/t.αH3PO4:4.0Kg/t.αH969:3.0Kg/t.α精矿64.7434.411.4582.4917.67尾矿35.2613.4212.4117.5182.33原矿100.0027.015.32100.00100.002#油:4滴H2SO4:1.0Kg/t.αH3PO4:4.0Kg/t.α2XP-64:3.0Kg/t.α精矿63.6634.631.0582.2112.76尾矿36.3413.1312.6017.7987.24原矿100.0026.825.25100.00100.002#油:4滴H2SO4:1.0Kg/t.αH3PO4:4.0Kg/t.α花王:3.0Kg/t.α精矿63.8333.432.1678.2325.99尾矿36.1716.4310.8721.7774.01原矿100.0027.285.31100.00100.006八、结论及建议:1.四川会东热水塘磷矿经过反浮选选矿试验,可以将P2O5品位从27.20%提高到34.05%,MgO品位从5.37%降到1.71%,精矿回收率89.70%,除镁率:76.30%。2.试验(二)原矿粒级筛析表明:-400目粒级MgO品位最高为7.46%,其次-320+400目粒级MgO品位为6.42%,说明镁结晶较细;-100+200目粒级P2O5品位31.52%最高,磷矿物结晶较粗,-320目粒级磷矿物单体部分过磨;磨矿细度-200目占73.00%时单体解离较完全。3.该磷矿石可选性较好,原矿P2O5品位27.20%偏低,MgO品位5.37%含量较高;原矿石为原生矿,磷矿物单体结晶较粗,而杂质镁的单体结晶较细,生产时磨矿不能过细,否则药剂的选择性下降易导致精矿氧化镁的含量偏高,除镁不理想。7四川会东热水塘磷矿石反浮选试验报告矿山生产技术处选矿实验室2010年4月28日
本文标题:四川会东磷矿石反浮选试验
链接地址:https://www.777doc.com/doc-322771 .html